中空玻璃打膠機(jī)膠槍堵塞的解決方案!
中空玻璃膠槍膠槍卡殼的解決方案,要進(jìn)行故障排除,有針對(duì)性地進(jìn)行解決。
To solve the problem of the shell of the glue gun of the hollow glass glue gun, we must first remove the trouble and solve it pertinently.
主要問題如下:
The main problems are as follows:
膠粘劑氧化引起的堵塞。
First adhesive oxidation caused by plugging.
第二膠中雜質(zhì)太多
Too many impurities in the second glue
第三,它沒有被清理
Third, it has not been cleaned up
隨著市場(chǎng)競(jìng)爭(zhēng)的日益激烈,一些廠家使用含有大量雜質(zhì)的劣質(zhì)硅膠膠,長(zhǎng)期使用導(dǎo)致中空玻璃膠機(jī)膠槍堵塞,該怎么辦?
With the increasingly fierce market competition, some manufacturers use a lot of impurities in the poor quality silica gel glue, long-term use leads to the blocking of hollow glass glue machine gun, what should be done?
中空玻璃打漿機(jī)膠槍堵塞原因:
Reasons for blocking of glue gun of hollow glass beater:
1. 在上膠過程中,中間中斷時(shí)間長(zhǎng),或累計(jì)多次,施膠結(jié)束時(shí)清洗不徹底,特別是在夏季溫度較高時(shí),膠水固化快。
1. In the process of sizing, the intermediate interruption time is long, or accumulated many times, and the cleaning is not complete at the end of sizing, especially in summer when the temperature is high, the glue solidifies quickly.
2. AB組分氣壓不足,混合不均勻,出膠慢,容易產(chǎn)生顆粒。
2. The air pressure of AB component is insufficient, the mixture is uneven, the glue is slow, and particles are easy to be produced.
3.B組件沒有檢查和清潔。B組分對(duì)水蒸氣很敏感。由于運(yùn)輸、儲(chǔ)存環(huán)境等偶發(fā)因素,B組分的結(jié)皮可能發(fā)生在表面,當(dāng)結(jié)皮部分被壓入管道時(shí),容易產(chǎn)生顆粒
3. B components are not inspected and cleaned. Component B is very sensitive to water vapor. Due to the occasional factors such as transportation and storage environment, the crust of component B may occur on the surface, and when the crust part is pressed into the pipeline, it is easy to produce particles

4. 濾網(wǎng)和單向止回閥很久沒有清洗了。
4. The filter screen and check valve have not been cleaned for a long time.
5. B組件壓力板上的o形環(huán)使用時(shí)間長(zhǎng),已經(jīng)松動(dòng)。
5. The O-ring on the pressure plate of B-component has been loose for a long time.
中空玻璃膠機(jī)膠槍堵塞解決方案:
Solution for blocking the glue gun of hollow glass glue machine:
1 .膠料的斷膠時(shí)間應(yīng)多長(zhǎng),建議在斷膠前,斷膠時(shí)間應(yīng)根據(jù)每天前不同的溫度和濕度而定。另外,現(xiàn)在客戶經(jīng)常要求膠液固化時(shí)間快,中斷時(shí)間長(zhǎng)一點(diǎn)容易造成顆粒的出現(xiàn)。
1. How long should the breaking time of rubber compound be? It is suggested that before breaking, the breaking time should be determined according to the different temperature and humidity of the day before each day. In addition, customers often require fast curing time and longer interruption time, which is easy to cause particles.
2 .簡(jiǎn)單處理是用刮板刮去外殼,不影響膠水的使用。
2. The simple treatment is to scrape off the shell with a scraper without affecting the use of glue.
建議定期清洗過濾器、單向止回閥、靜電混合器和膠槍。
It is recommended to clean the filter, one-way check valve, electrostatic mixer and glue gun regularly.